| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.08 g/cc | 0.0390 lb/in³ | DAM; ISO 1183 |
| Water Absorption | 1.1 % @Temperature 23.0 °C |
1.1 % @Temperature 73.4 °F |
DAM; Immersion 24h; ISO 62, Similar to |
| 6.7 % @Temperature 23.0 °C |
6.7 % @Temperature 73.4 °F |
DAM; Saturation, immersed; ISO 62, Similar to | |
| 2.0 % @Thickness 1.00 mm, Temperature 23.0 °C |
2.0 % @Thickness 0.0394 in, Temperature 73.4 °F |
DAM; Equilibrium 50%RH; ISO 62, Similar to | |
| Linear Mold Shrinkage, Flow | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Stress | 45.0 MPa @Strain 50.0 %, Temperature 23.0 °C |
6530 psi @Strain 50.0 %, Temperature 73.4 °F |
50%RH; ISO 527 |
| 52.0 MPa @Strain 50.0 %, Temperature 23.0 °C |
7540 psi @Strain 50.0 %, Temperature 73.4 °F |
DAM; ISO 527 | |
| Tensile Strength, Yield | 39.0 MPa @Temperature 23.0 °C |
5660 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 52.0 MPa @Temperature 23.0 °C |
7540 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Elongation at Break | 47 % @Temperature 23.0 °C |
47 % @Temperature 73.4 °F |
DAM; ISO 527 |
| >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| Elongation at Yield | 4.0 % @Temperature 23.0 °C |
4.0 % @Temperature 73.4 °F |
DAM; ISO 527 |
| >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| Tensile Modulus | 0.910 GPa @Temperature 23.0 °C |
132 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 2.00 GPa @Temperature 23.0 °C |
290 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Flexural Modulus | 0.823 GPa @Temperature 23.0 °C |
119 ksi @Temperature 73.4 °F |
50%RH; ISO 178 |
| 1.89 GPa @Temperature 23.0 °C |
274 ksi @Temperature 73.4 °F |
DAM; ISO 178 | |
| Izod Impact, Notched (ISO) | 14.0 kJ/m² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
DAM; ISO 180/1A |
| 16.0 kJ/m² @Temperature -40.0 °C |
7.61 ft-lb/in² @Temperature -40.0 °F |
50%RH; ISO 180/1A | |
| 19.0 kJ/m² @Temperature -40.0 °C |
9.04 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A | |
| 20.0 kJ/m² @Temperature -20.0 °C |
9.52 ft-lb/in² @Temperature -4.00 °F |
50%RH; ISO 180/1A | |
| 76.0 kJ/m² @Temperature 23.0 °C |
36.2 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
| 94.0 kJ/m² @Temperature 23.0 °C |
44.7 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A | |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
DAM; ISO 179/1eU | |
| Charpy Impact, Notched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
| 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA | |
| 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ASTM E 831 |
| 80.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 | |
| 80.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ISO 11359-1/-2 | |
| 80.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 | |
| 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 | |
| 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 100 µm/m-°C @Temperature 55.0 - 160 °C |
55.6 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 | |
| 100 µm/m-°C @Temperature 55.0 - 160 °C |
55.6 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| CTE, linear, Transverse to Flow | 100 µm/m-°C @Temperature -30.0 - 30.0 °C |
55.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ISO 11359-1/-2 |
| 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 | |
| 100 µm/m-°C @Temperature -30.0 - 30.0 °C |
55.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ASTM E 831 | |
| 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 | |
| 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 | |
| 150 µm/m-°C @Temperature 55.0 - 160 °C |
83.3 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 | |
| 150 µm/m-°C @Temperature 55.0 - 160 °C |
83.3 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 157 °C | 315 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | DAM; ISO 75-1/-2 |
| Glass Transition Temp, Tg | 75.0 °C | 167 °F | DAM; 10°C/min; ISO 11357-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.70e+12 ohm-cm @Temperature 23.0 °C |
2.70e+12 ohm-cm @Temperature 73.4 °F |
50%RH; IEC 60093 |
| 1.80e+16 ohm-cm @Temperature 23.0 °C |
1.80e+16 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 | |
| Surface Resistance | 5.00e+12 ohm @Temperature 23.0 °C |
5.00e+12 ohm @Temperature 73.4 °F |
50%RH; IEC 60093 |
| 3.00e+15 ohm @Temperature 23.0 °C |
3.00e+15 ohm @Temperature 73.4 °F |
DAM; IEC 60093 | |
| Dielectric Constant | 3.3 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
3.3 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
DAM; IEC 60250 |
| 3.5 @Frequency 100 Hz, Temperature 23.0 °C |
3.5 @Frequency 100 Hz, Temperature 73.4 °F |
DAM; IEC 60250 | |
| 3.6 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
3.6 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
50%RH; IEC 60250 | |
| 6.2 @Frequency 100 Hz, Temperature 23.0 °C |
6.2 @Frequency 100 Hz, Temperature 73.4 °F |
50%RH; IEC 60250 | |
| Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm, Temperature 23.0 °C |
610 kV/in @Thickness 0.0787 in, Temperature 73.4 °F |
50%RH; IEC 60243-1 |
| 24.0 kV/mm @Thickness 2.00 mm, Temperature 23.0 °C |
610 kV/in @Thickness 0.0787 in, Temperature 73.4 °F |
DAM; IEC 60243-1 | |
| Dissipation Factor | 0.0050 @Frequency 100 Hz, Temperature 23.0 °C |
0.0050 @Frequency 100 Hz, Temperature 73.4 °F |
DAM; IEC 60250 |
| 0.011 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
0.011 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
DAM; IEC 60250 | |
| 0.040 @Frequency 1.00e+6 Hz, Temperature 23.0 °C |
0.040 @Frequency 1.00e+6 Hz, Temperature 73.4 °F |
50%RH; IEC 60250 | |
| 0.177 @Frequency 100 Hz, Temperature 23.0 °C |
0.177 @Frequency 100 Hz, Temperature 73.4 °F |
50%RH; IEC 60250 | |
| Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; IEC 60112 |
| >= 600 V @Thickness 3.00 mm, Temperature 23.0 °C |
>= 600 V @Thickness 0.118 in, Temperature 73.4 °F |
50%RH; UL 746A |