Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 165 - 168 °C | 329 - 334 °F | ASTM D3418 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Melting Point | 162 - 168 °C | 324 - 334 °F | Sheath Melt Point; LCL-PR29 |
Intercontinental Polymers 1180 Bicomponent PP/PET Fiber Type - 3 Denier X 1.5 Inches 40/60 PP Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdenier.. |
|||
Melting Point | 162 - 168 °C | 324 - 334 °F | DSC |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53... |
|||
Melting Point | 164 - 168 °C | 327 - 334 °F | DSC; ISO 3146 |
Borealis HB300TF Polypropylene HB300TF is a polypropylene homopolymer intended for thermoformed packaging applications. This grade is produced using the Borealis nucleating technology. Its increased crystallization temperature a.. |
|||
Melting Point | 164 - 168 °C | 327 - 334 °F | ISO 1218 Method A; DIN 53736 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) at 50% RH Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction prope.. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 140 Polypropylene Homopolymer Unreinforced, low flow for injection and extrusion, very translucentInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 210 G20 Polypropylene Homopolymer Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 211 V20 Polypropylene Homopolymer Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 220 M40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 526 N30 Polypropylene Homopolymer Improved rigidity, high durabilityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 530 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 555 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 560 Polypropylene Homopolymer High heat resistance, detergent stabilized, anti-yellowingInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 652 Polypropylene Homopolymer High temperature resistance, high gloss, very good surface appearanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 120 M10 Polypropylene Copolymer Low fluidity for extrusion or injectionInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 370 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 522 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 522 N30 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 690 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50215 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50272 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 511 V30 Polypropylene Homopolymer Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 430 N30 Polypropylene Copolymer Good surface appearanceInformation provided by Addiplast. |
|||
Melting Point | 162 - 168 °C | 324 - 334 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50291 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Melting Point | 145 - 168 °C | 293 - 334 °F | Average value: 161 °C Grade Count:8 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Melting Point | 160 - 168 °C | 320 - 334 °F | 10°C/min; ASTM D3418 |
Shanghai Ofluorine 904 PVDF for water UF (ultrafiltration) Membranes Description: Ofluorine 904 PVDF Powder for water UF membranes has good solubility in some special solvent, which is a good raw material for PVDF UF membranes. Ofluorine 904 PVDF as raw materials, th.. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50265 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Melting Point | 160 - 168 °C | 320 - 334 °F | Average value: 164 °C Grade Count:47 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |