Shanghai Ofluorine 904 PVDF for water UF (ultrafiltration) Membranes

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Shanghai Ofluorine
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shanghai Ofluorine 904 PVDF for water UF (ultrafiltration) Membranes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ofluorine 904 PVDF Powder for water UF membranes has good solubility in some special solvent, which is a good raw material for PVDF UF membranes. Ofluorine 904 PVDF as raw materials, the PVDF membranes has excellent mechanical strength and flexibility. It can not be eroded by acid, alkali, strong oxidant, halogens. Good durability to aliphatic hydrocarbons, aromatic hydrocarbons, alcohol, aldehyde etc. In the work of hydrochloric acid, nitric acid, sulfuric acid, dilute alkali liquor, dense alkali liquor (40%) and 100°C, which keep stable. Others, 904 PVDF finished products has the properties of gamma-Ray resistant, UV (ultraviolet) resistant, and stability in wide temperature range.Information provided by Shanghai Ofluorine Chemical Technology
Physical Properties Metric English Comments
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Water Absorption 0.10 %
0.10 %
Drying loss method
Viscosity Measurement 1.4 - 1.9
1.4 - 1.9
[10<sup>2</sup> ml/g], Intrinsic Viscosity
>= 0.45

@Temperature 30.0 °C
>= 0.45

@Temperature 86.0 °F
[mPa.S] 1g/ml MNP, Rotary Viscosity
Thermal Properties Metric English Comments
Melting Point 160 - 168 °C
320 - 334 °F
10°C/min; ASTM D3418
Descriptive Properties Value Comments
Appearance White powder
Solubility Solution is clear and transparent, no impurity and insoluble matter