Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 340 °C | 644 °F | |
Oceanchem Group Decabromodiphenyl Ethane (DBDPE/8010) Molecular Formula: C14Br10H4Cas No.: 84852-53-9Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: This.. |
|||
Melting Point | 340 °C | 644 °F | ISO 11357 |
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet) KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. .. |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Melting Point | 340 - 372 °C | 644 - 702 °F | Average value: 347 °C Grade Count:6 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Melting Point | 340 - 360 °C | 644 - 680 °F | Average value: 350 °C Grade Count:8 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard.. |
|||
Melting Point | >= 340 °C | >= 644 °F | ISO 3146 |
Panjin Zhongrun Chemerize 012G High Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers Ajedium™ KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK) KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK) KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK) KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Melting Point | 340 °C | 644 °F | DSC, Second Heating; ISO 11357 |
Westlake Plastics MediPEEK IM Polyetheretherketone for Medical Applications MediPEEK-IM is a high performance semi-crystalline thermoplastic designed for long term body contact as an implantable material. It is USP Class VI and compliant to ASTM F2026. It has excellent st.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Melting Point | 340 °C | 644 °F | |
Ensinger Tecapeek® MT Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Melting Point | 340 °C | 644 °F | |
Ensinger Tecapeek® Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Melting Point | 340 °C | 644 °F | ISO 11357-1 |
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Gharda Chemicals GATONE™ 5300PF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Melting Point | >= 340 °C | >= 644 °F | ISO 3146 |
Panjin Zhongrun Chemerize 085G Low Viscosity CoPEEK Information provided by Bieglo Gmbh. |