Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Water Absorption | 0.18 % | 0.18 % | Immersion, 24hr; ASTM D570(2) |
Water Absorption at Saturation | 1.65 % | 1.65 % | Immersion; ASTM D570(2) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 105 | 105 | ASTM D785 |
Hardness, Rockwell R | 123 | 123 | ASTM D785 |
Tensile Strength | 96.5 MPa | 14000 psi | ASTM D638 |
Elongation at Break | 2.3 % | 2.3 % | ASTM D638 |
Tensile Modulus | 6.48 GPa | 940 ksi | ASTM D638 |
Flexural Strength | 145 MPa | 21000 psi | ASTM D790 |
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Compressive Strength | 179 MPa | 26000 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 4.14 GPa | 600 ksi | ASTM D695 |
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 Type A |
Coefficient of Friction, Dynamic | 0.20 | 0.20 | Dry vs. Steel; QTM55007 |
Limiting Pressure Velocity | 0.596 MPa-m/sec | 17000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 50.4 µm/m-°C @Temperature -40.0 - 149 °C |
28.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Maximum Service Temperature, Air | 246 °C | 475 °F | Long Term |
Deflection Temperature at 1.8 MPa (264 psi) | 260 °C | 500 °F | ASTM D648 |
Flammability, UL94 | V-0 | V-0 | 1/8 inch (Estimated Rating) |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | EOS/ESD S11.11 |
Dielectric Constant | 5.33 @Frequency 1e+6 Hz |
5.33 @Frequency 1e+6 Hz |
ASTM D150 |
Dissipation Factor | 0.227 @Frequency 1e+6 Hz |
0.227 @Frequency 1e+6 Hz |
ASTM D150 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | No | No | |
Canada AG | No | No | |
FDA | No | No | |
NSF | No | No | |
USDA | No | No | |
USP Class VI | No | No |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Limited | Limited | |
Acids, Weak | Acceptable | Acceptable | |
Alcohols | Acceptable | Acceptable | |
Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
Alkalies, Weak | Limited | Limited | |
Chlorinated Solvents | Acceptable | Acceptable | |
Conductive / Static Dissipative | Yes | Yes | |
Continuous Sunlight | Acceptable | Acceptable | |
Hot Water / Steam | Acceptable | Acceptable | |
Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
Hydrocarbons - Aromatic | Acceptable | Acceptable | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Acceptable | Acceptable |
Descriptive Properties | Value | Comments |
---|---|---|
Machinability | 4 | 1-10, 1=Easier to Machine |