Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyketone , Polyaryletherketone (PAEK), Carbon Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wear resistance, the resin also offers the outstanding combination of ultra performance attributes commonly known for PEEK. These include: chemical resistance, mechanical strength and stiffness, even at elevated temperatures, as well as long-term and high-temperature thermal-oxidative stability. AV-722 SL30 is formulated with the ternary anti-friction/anti-wear additive system comprised of carbon fiber, graphite, and polytetrafluoroethylene (PTFE.) It offers wear resistance performance comparable to PEEK grades with this modifier system while being more cost-effective. This resin is a low melt flow (high viscosity) grade designed for use in injection molding of less intricate shapes or parts. By virtue of its high viscosity at low shear rates, the resin has high melt strength, and, as such, is extrudable into stock shapes such as rods, pipe, tubing and profile. The resin can be melt processed using conventional equipment and techniques. Potential applications for AV-722 SL30 include bushings, bearings, wear strips, wear rings, rollers, and other parts or components where sliding friction is encountered. The resin is black in color in its natural state.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Water Absorption 0.030 %

@Time 86400 sec
0.030 %

@Time 24.0 hour
ASTM D570
Viscosity 240000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
240000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Thickness 3.18 mm
0.0010 - 0.0030 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125" bars; ASTM D955
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm

@Thickness 3.18 mm
0.017 - 0.019 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125" bars; ASTM D955
Melt Flow 1.9 g/10 min
1.9 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 82
82
M-Scale; ASTM D785
Tensile Strength 136 MPa
19700 psi
5.0 mm/min; ASTM D638
Tensile Strength, Yield 151 MPa
21900 psi
ISO 527-2/1A/5
Elongation at Break 2.1 %
2.1 %
5.0 mm/min; ASTM D638
2.1 %
2.1 %
ISO 527-2/1A/5
Tensile Modulus 12.4 GPa
1800 ksi
5.0 mm/min; ASTM D638
15.7 GPa
2280 ksi
ISO 527-2/1A/1
Flexural Strength 209 MPa
30300 psi
ISO 178
213 MPa
30900 psi
ASTM D790
Flexural Modulus 10.2 GPa
1480 ksi
ASTM D790
13.9 GPa
2020 ksi
ISO 178
Compressive Strength 107 MPa
15500 psi
ASTM D695
Shear Strength 71.0 MPa
10300 psi
ASTM D732
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
4.50 J/cm
8.43 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 7.40 kJ/m²
3.52 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
ISO 180
Coefficient of Friction, Dynamic 0.080
0.080
Lubricated conditions: 800 fpm and 750 psi; ASTM D3702
0.11
0.11
Lubricated conditions: 75 fpm and 1000 psi; ASTM D3702
0.42
0.42
Dry conditions: 800 fpm and 31.25 psi; ASTM D3702
0.59
0.59
Dry conditions: 200 fpm and 125 psi; ASTM D3702
Thermal Properties Metric English Comments
Specific Heat Capacity 1.34 J/g-°C

@Temperature 50.0 °C
0.320 BTU/lb-°F

@Temperature 122 °F
DSC
1.81 J/g-°C

@Temperature 200 °C
0.433 BTU/lb-°F

@Temperature 392 °F
DSC
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
ASTM E1530
Melting Point 340 °C
644 °F
Peak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 267 °C

@Thickness 3.20 mm
513 °F

@Thickness 0.126 in
Annealed; 2 hours at 200°C; ASTM D648
Glass Transition Temp, Tg 152 °C
306 °F
DSC
Processing Properties Metric English Comments
Rear Barrel Temperature 354 °C
669 °F
Middle Barrel Temperature 366 °C
691 °F
Front Barrel Temperature 371 °C
700 °F
Nozzle Temperature 374 °C
705 °F
Melt Temperature 366 - 388 °C
691 - 730 °F
Mold Temperature 149 - 177 °C
300 - 351 °F
Drying Temperature 149 °C
300 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Additive Carbon Fiber + Graphite + PTFE Lubricant
Appearance Black
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Flame Retardant
Good Chemical Resistance
Good Dimensional Stability
Good Wear Resistance
High Heat Resistance
Forms Pellets
Generic PAEK
Injection Rate Fast
Processing Method Injection Molding
Machining
Profile Extrusion
Screw Compression Ratio 2.0:1.0 to 3.0:1.0
Uses Automotive Applications
Bearings
Bushings
Oil/Gas Applications
Wear Strip
Users viewing this material also viewed the following: