Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Solvay Specialty Polymers
Trade Name KetaSpire®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical properties at temperatures approaching 300°C, and the lowest coefficient of linear thermal expansion within the KetaSpire® product family.KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity, and excellent chemical resistance to organics, acids and bases. Features: Autoclave Sterilizable; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; Good Sterilizability; Heat Sterilizable; High Heat Resistance; High Stiffness; High Strength; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam SterilizableUses: Automotive Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Gears; Hospital Goods; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Oil/Gas Applications; Pump Parts; Surgical Instruments; Thrust WasherInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Filler Content 30 %
30 %
Carbon Fiber
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ISO 62
Viscosity 920000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
920000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Linear Mold Shrinkage, Flow 0.00 - 0.0020 cm/cm

@Thickness 3.18 mm
0.00 - 0.0020 in/in

@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Thickness 3.18 mm
0.015 - 0.017 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 1.1 g/10 min

@Load 2.16 kg,
Temperature 400 °C
1.1 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 105
105
ASTM D785
Hardness, Shore D 92
92
1 sec; ASTM D2240
Tensile Strength 201 MPa
29200 psi
ASTM D638
Tensile Strength, Yield 217 MPa
31500 psi
5 mm/min, Type 1A; ISO 527-2
Elongation at Break 2.0 %
2.0 %
Type 1A, 5 mm/min; ISO 527-2
2.0 %
2.0 %
5 mm/min; ASTM D638
Tensile Modulus 19.7 GPa
2860 ksi
5 mm/min; ASTM D638
22.8 GPa
3310 ksi
1 mm/min, Type 1A; ISO 527-2
Flexural Strength 311 MPa
45100 psi
ISO 178
317 MPa
46000 psi
ASTM D790
Flexural Modulus 17.5 GPa
2540 ksi
ASTM D790
20.5 GPa
2970 ksi
ISO 178
Compressive Strength 173 MPa
25100 psi
ASTM D695
Poissons Ratio 0.42
0.42
ASTM E132
Shear Strength 95.1 MPa
13800 psi
ASTM D732
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.50 J/cm
14.1 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) 44.0 kJ/m²
20.9 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 5.20 µm/m-°C

@Temperature -50.0 - 50.0 °C
2.89 µin/in-°F

@Temperature -58.0 - 122 °F
1
Specific Heat Capacity 1.13 J/g-°C

@Temperature 50.0 °C
0.270 BTU/lb-°F

@Temperature 122 °F
ASTM C351
1.62 J/g-°C

@Temperature 200 °C
0.387 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Thermal Conductivity 0.370 W/m-K
2.57 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 340 °C
644 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Annealed; ASTM D648
Glass Transition Temp, Tg 150 °C
302 °F
DSC
Flammability, UL94 V-0

@Thickness 0.800 - 1.60 mm
V-0

@Thickness 0.0315 - 0.0630 in
Processing Properties Metric English Comments
Rear Barrel Temperature 365 °C
689 °F
Middle Barrel Temperature 370 °C
698 °F
Front Barrel Temperature 375 °C
707 °F
Nozzle Temperature 380 °C
716 °F
Mold Temperature 175 - 205 °C
347 - 401 °F
Drying Temperature 150 °C

@Time 14400 sec
302 °F

@Time 4.00 hour
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
Injection Rate Fast
Processing Technique Injection Molding; Machining; Profile Extrusion
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.5:1.0 to 3.5:1.0