Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 256 °C | 493 °F | ASTM D789 |
PolyOne Nymax™ 1200 A HS Natural A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Melting Point | 256 °C | 493 °F | @ 15°C/min; ASTM D3418 |
Ovation Polymers Opnyl OP66UT105 Nylon 66 Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All.. |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 H-SG50 Nylon 6.6 for injection molding, 50% mineral filled Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 S Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 TF30 Nylon 6.6 for injection molding, 30% PTFE lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 W-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit RECONYL A H Recycled nylon 6.6 for injection molding Recycled nylon 6.6 for injection molding, heat stabilized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 H-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 H-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 HS-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 KF30 M2 Nylon 6.6 for injection molding, 30% short glass fiber reinforced and 2% molybdenum disulphide lubricated Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | ISO 3146 DSC |
Nilit FRIANYL A63 KV40 Nylon 6.6 for injection molding, 40% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek PA301G50 Nylon 6.6, Heat Stabilized, 50% Glass Fiber Heat stabilized, 50% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek PA303G5 Nylon 6.6, 25% Glass Fiber 25% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | ISO 11357 |
Polyram PlusTek PA700BL10 Nylon 6.6 for Injection Molding, UV Stabilized UV Stabilized Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek PA830 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek PA880 Nylon 6.6, Impact Modified Super tough - impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek RA325J5 Nylon 6.6, 25% Glass beads and Glass Fiber, Flame Retardant 25% glass beads and glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | DSC |
Polyram Polytron A30B041 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek RA124 Nylon 6.6, Injection Molding Fast cycle polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek RA301G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | ISO 11357 |
Polyram PlusTek RA301G8 Nylon 6.6 for Injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 40% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek RA303G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized, and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek RA307G4 Nylon 6.6, 20% Glass Fiber 20% glass fiber reinforced heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram RamLloy PA917G6 PP/NYLON 66 alloy, 30% Glass Fiber 30% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 256 °C | 493 °F | |
DuPont Teijin Films Melinex® ST505 Polyester Film, 500 Gauge Melinex® ST505 is a crystal clear, high gloss, heat stabilized polyester film. It is pretreated on both sides for improved adhesion. It can be overprinted with a wide range of solvent-based graphic.. |
|||
Melting Point | 256 °C | 493 °F | |
Polyram PlusTek RA320G3 Nylon 6.6, 15% Glass Fiber, Flame Retardant 15% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |