Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 255 °C | 491 °F | ASTM D1525 |
Kolon KOPA® KN333HRBL Heat Resistant Nylon 66 Middle viscosity, BLACKApplications A variety of reservoir tanks and housingsInformation provided by API-Kolon. |
|||
Melting Point | 255 °C | 491 °F | |
Solvay Technyl® A218 Heat Stabilized Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
Shandong Dongyue Shenzhou New Material Co DS602 Perfluorinated Ethylene-Propylene Copolymer Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and.. |
|||
Melting Point | 255 °C | 491 °F | ISO 1218 Method A; DIN 53736 |
Zell-Metall Engineering Plastics Zellamid 1400 (PET) at 50% RH Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Melting Point | 255 °C | 491 °F | DSC |
Toyobo Vylopet® EMC605 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: glossy surface componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanic.. |
|||
Melting Point | 255 °C | 491 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnite® AV2 390 PET-50% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Melting Point | 255 °C | 491 °F | Kofler |
CP-Polymer-Technik Wellamid® 6600 GS 20 HWCP 20% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melting Point | 255 °C | 491 °F | Kofler |
CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melting Point | 255 °C | 491 °F | Kofler |
CP-Polymer-Technik Wellamid® 6600/506 HWCP Nylon 66, Impact Modified, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melting Point | 255 °C | 491 °F | ASTM D2133 |
Ensinger Tecamid® MDS® Molybdenum Disulfide Filled Nylon (PA) Tecamid MDS® has enhanced surface lubricity and wear resistance over unfilled nylon. It is an ideal material to replace metals in machinery. Low surface friction Increased surface hardness Incre.. |
|||
Melting Point | <= 255 °C | <= 491 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 6100.17 Linear Low Density Polyethylene Resin Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in .. |
|||
Melting Point | 255 °C | 491 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT70 GR30 NL100 MB PET, 30% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 255 - 260 °C | 491 - 500 °F | ASTM E794-85 |
DuPont Teijin Films Melinex® 542 Polyester Film Melinex® 542 is a slightly hazy film with an adhesion promoting pretreatment on both sidesGeneral Product Info: The pretreatment enables numerous solvent and UV inks and lacquers to be coated with .. |
|||
Melting Point | 255 °C | 491 °F | [10 K/min], ISO 11357 |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 255 °C | 491 °F | ASTM D789 |
Adell AJ-13 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Melting Point | 255 °C | 491 °F | ISO 11357-1, DSC,10 [K/min] |
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Melting Point | 255 °C | 491 °F | ISO 11357-1, DSC,10 [K/min] |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Melting Point | 255 °C | 491 °F | ASTM D4591 |
3M Dyneon™ FEP 6322Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6322Z was designed primarily for high-speed extrusion for wire insulation. Its distinguishing features include:High extrusion speedHigh thermal stabilityWide processing windowSuperior ele.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Comtuf® 607 Nylon 6/6, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Comtuf® 635 Nylon 6/6, Glass/Mineral Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has .. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Comtuf® 639 Nylon 6/6, Mineral Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Mineral reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 622 Nylon 6/6, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Voloy® 630 Nylon 6/6, Flow Enhanced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
A. Schulman ComAlloy Voloy® 685 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.48% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Melting Point | 255 °C | 491 °F | ASTM D789 |
Adell AT-17 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Melting Point | 255 °C | 491 °F | ASTM D3418 |
Ashley Polymers Ashlene® R528LW Nylon 66 General purpose injection molding grade Nylon 66, lubricated and FDA approved.Data provided by the manufacturer |
|||
Melting Point | 255 - 263 °C | 491 - 505 °F | Average value: 259 °C Grade Count:11 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Melting Point | 255 - 275 °C | 491 - 527 °F | |
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff.. |