| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant |
| Manufacturer | Ashley Polymers |
| Trade Name | Ashlene® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Ashley Polymers Ashlene® R528LW Nylon 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
| Water Absorption | 1.35 % | 1.35 % | 24 hrs; ASTM D570 |
| Moisture Absorption at Equilibrium | 2.2 % | 2.2 % | ASTM D570 |
| Water Absorption at Saturation | 8.6 % | 8.6 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 104 | 104 | ASTM D785 |
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | ASTM D638 |
| Tensile Modulus | 1.435 GPa | 208.1 ksi | ASTM D638 |
| Flexural Strength | 51.0 MPa | 7400 psi | ASTM D790 |
| Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 |
| Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 255 °C | 491 °F | ASTM D3418 |
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous Service temperature. |
| Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 82.0 °C | 180 °F | ASTM D648 |
| Flammability, UL94 | V-2 | V-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.2 @Frequency 1e+6 Hz |
3.2 @Frequency 1e+6 Hz |
ASTM D150 |