Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion

Category Polymer , Thermoplastic , Fluoropolymer , FEP
Manufacturer Shandong Dongyue Shenzhou New Material Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coefficient of friction, enabling thermoplastic processing methods. DS608 are high molecular weight resins of low melt index, with low extrusion temperature, high extrusion speed which is 5 ~ 8 times of ordinary FEP resin. It is soft, anti-burst, and has good toughness.Main Applications:Mainly for aviation and aerospace industry, the MTR transport vehicles, automatic switching equipment, well test equipment, flame alarm systems, high-rise buildings, fire regional wires, cables, computers, communication networks, electrical fields, particularly applicable for high-speed extrusion small-caliber wire insulation material. It is more economical when used where no high stress cracking resistance is required.Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 2.14 - 2.17 g/cc
2.14 - 2.17 g/cc
Volatiles <= 0.10 %
<= 0.10 %
Melt Flow 12.1 - 16 g/10 min
12.1 - 16 g/10 min
D
16.1 - 20 g/10 min
16.1 - 20 g/10 min
A
20.1 - 24 g/10 min
20.1 - 24 g/10 min
B
24.1 - 28 g/10 min
24.1 - 28 g/10 min
C
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 16.0 MPa
>= 2320 psi
>= 18.0 MPa
>= 2610 psi
>= 20.0 MPa
>= 2900 psi
>= 20.0 MPa
>= 2900 psi
Elongation at Break >= 250 %
>= 250 %
>= 270 %
>= 270 %
>= 300 %
>= 300 %
>= 300 %
>= 300 %
Thermal Properties Metric English Comments
Melting Point 255 - 275 °C
491 - 527 °F
Electrical Properties Metric English Comments
Dielectric Constant <= 2.15

@Frequency 1.00e+6 Hz
<= 2.15

@Frequency 1.00e+6 Hz
Dissipation Factor <= 0.00070

@Frequency 1.00e+6 Hz
<= 0.00070

@Frequency 1.00e+6 Hz
Descriptive Properties Value Comments
Appearance Translucent particles, without impurities such as metal debris and sand, containing visible black particles less than 2%