Polymer Property : CTE, linear, Parallel to Flow = 75.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature -40.0 - 60.0 °C
75.0 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® BDT5510 ABS
Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade
Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats..
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
Covestro Baydur® GS PUR Polyurethane
Polyurethane casting system for the production of solid components. Pressureless casting into open or closed molds, fast demold times, good rot resistance. Combines easily with other materials.Infor..
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1040 K Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1040 N Polypropylene
Nucleated grade for injection molded parts.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade
Injection moldingsData was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade
Injection molded parts, film tape, fibrillated film and monofilaments.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1101 M Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1101 P Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1101 R Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1102 G Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1102 H Polypropylene
Grade with high processing stability for packaging tapes, film tape, fibrillated film, monofilaments, thermoformed and blow molded parts.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1102 M Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1100 N Polypropylene, Injection Molding Grade
Grade for injection molded parts. Also available as a special grade for fibers (short spinning) and cast film.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1100 VC Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1101 N Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1102 J Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1102 L Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1104 K Polypropylene
Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1125 N Polypropylene
Cast film with medium slip.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1126 N Polypropylene
Grade with slip and antiblocking agents, for cast and water-cooled blown film with very good slip and especially low tendency to block.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1127 N Polypropylene
Grade with slip and antiblocking agents, for cast film; with very good slip.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1148 RC Polypropylene
Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1148 TC Polypropylene
Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
BASF Novolen® 1148 UC Polypropylene
Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF.
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
ASTM D636
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in..
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.