Material Notes:
Cast film with medium slip.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
Water Absorption 0.10 %
0.10 %
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
Melting Point 163 °C
325 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
Dielectric Strength 140 kV/mm
3560 kV/in
Dissipation Factor 0.000070

@Frequency 100 Hz
0.000070

@Frequency 100 Hz
0.00020

@Frequency 1e+6 Hz
0.00020

@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
600 V