Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants 2000 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants 363P (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants 365FT (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants 868VL (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants UniFlor 8140 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants UniFlor 8520 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants UniFlor 8521BL (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E70V Ethylene Propylene Rubber Peroxide cured, blue-violet Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage .. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Parker Chomerics CHO-BOND SV713 Conductive Epoxy CHO-BOND® 700 Series Adhesives for Microelectronics Packaging; these pure silver-filled epoxy pastes are designed to meet the demanding requirements of semiconductor and microelectronic packaging. .. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and c.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Parker Chomerics Waveguide Gaskets 877 Conductive Silicone Elastomer Gasket Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; EN 495-5 |
Lucobit Lucofin® 1415 Polyolefin TPO Granules, Signal White Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; EN 495-5 |
Lucobit Lucofin® 1453 Polyolefin TPO Granules, Red Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucofin® 1451 Polyolefin TPO Granules, Light Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Master Bond MasterSil 707FR Flame Retardant Silicone Adhesive Description: MasterSil 707FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V-1 for thicknesses of .. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning HM-2500 CLEAR ASSEMBLY SEALANT A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning SE 4490 CV One-part, white, non-flowing, highly filled compound, excellent thermal conductivity.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning SE 738 SILICONE RTV One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning SLYGARD® 535 THIXOTROPIC DIELECTRIC GEL Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
ChevronTexaco Delo® Synthetic Grease SF FeaturesChevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperature.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | JIS-K-6723 |
Denka REOMER G G3015 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning 3-4150 DIELECTRIC GEL KIT Two-part, transparent green, fast RT or heat cure.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning 3-4222 DIELECTRIC FIRM GEL KIT Two-part, translucent green, firm, fast RT or heat cure, and primerless chemical adhesion.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning 3-4680 SILICONE GEL KIT Two-part, transparent blue, fast RT or heat cure, low viscosity.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
ATG s.r.l. IR Synthetic Polyisoprene |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucolit® 1320 Polyolefin TPO Granules, Beige Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucofin® 1460 Polyolefin TPO Granules, White Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |