Polymer Property : Minimum Service Temperature, Air = -45.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Recommended
Nye Lubricants 274VL (SO) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Recommended
Nye Lubricants 363P (RL) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Recommended
Nye Lubricants 365F (RL) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Recommended
Nye Lubricants 868VL (FG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Recommended
Nye Lubricants UniFlor 8140 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Recommended
Nye Lubricants UniFlor 8160 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Recommended
Nye Lubricants UniFlor 8520 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Precision Polymer Engineering E65K Ethylene Propylene Rubber
Peroxide cured, Ethylene Propylene Terpolymer (EPT), 50-70 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing sulphur hexafluoride (SF6) gas in electric..
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering E80V Ethylene Propylene Rubber
Peroxide cured, blue-violet coloured Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high..
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Parker Chomerics CHO-BOND SV712 Conductive Epoxy
CHO-BOND® 700 Series Adhesives for Microelectronics Packaging; these pure silver-filled epoxy pastes are designed to meet the demanding requirements of semiconductor and microelectronic packaging. ..
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Flex TR10; ASTM D1329
Parker Chomerics CHO-SEAL 1212 Conductive Elastomer
High strength, hard (80 shore A) material for waveguide, choke, cover, and flanges with grooves for EMI and pressure sealing.Molded onlyRoHS Compliant Information provided by Chomerics
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Parker Chomerics CHO-SEAL E6306 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering E50E Ethylene Propylene Rubber
Ethylene Propylene Terpolymer, 46-55 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace Specification DTD5597A Grade 50.Applications: For sealing applications where goo..
Minimum Service Temperature, Air <= -45.0 °C
<= -49.0 °F
Low Temperature Flexural Test; EN 495-5
Lucobit Lucofin® 1413 Polyolefin TPO Granules, Dark Grey
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi..
Minimum Service Temperature, Air <= -45.0 °C
<= -49.0 °F
Low Temperature Flexural Test; DIN 53361
Lucobit Lucolit® 1322 Polyolefin TPO Granules, Red
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi..
Minimum Service Temperature, Air <= -45.0 °C
<= -49.0 °F
Low Temperature Flexural Test; DIN 53361
Lucobit Lucolit® 1323 Polyolefin TPO Granules, Green
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi..
Minimum Service Temperature, Air <= -45.0 °C
<= -49.0 °F
Low Temperature Flexural Test; DIN 53361
Lucobit Lucofin® 1452 Polyolefin TPO Granules, Blue
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi..
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Trelleborg R642 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Dow Corning CY 52-276 KIT
Two-part, clear, 1:1, addition cure, low temperature cure, low viscosity, controlled volatility.Information provided by Dow Corning
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Dow Corning SE 4430 KIT
Two-part, thermally conductive elastomer, soft, good thermal conducitvity, UL 94 V-0 rating, low viscosity.Information provided by Dow Corning
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Dow Corning SE 738 SILICONE RTV
One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB.Information provided by Dow Corning
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Dow Corning SE 9184 WHITE RTV
One-part, white, moisture cure RTV, non-flowing, fast tack free, controlled volatility, thermally conductive, UL V-0.Information provided by Dow Corning
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
JIS-K-6723
Denka REOMER G G3015 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Dow Corning 3-4133 DIELECTRIC GEL KIT
Two-part, clear, heat cure, and firm.Information provided by Dow Corning
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Dow Corning 3-4150 DIELECTRIC GEL KIT
Two-part, transparent green, fast RT or heat cure.Information provided by Dow Corning
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Dow Corning 3-4154 DIELECTRIC GEL KIT
Two-part, clear, RT or heat cure.Information provided by Dow Corning
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Dow Corning 3-4241 DIELECTRIC TOUGH GEL KIT
Two-part, translucent green, RT or heat cure, UV indicator, long working time, tough primerless chemical adhesion, UL 94 V-1 flammability classification.Information provided by Dow Corning
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Flex TR10
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer
Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Molded onlyRoHS CompliantInformation provided by Chomerics