Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants 2000 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants 365 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants 365FT (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E60E Ethylene Propylene Rubber Ethylene Propylene Terpolymer, 56-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace Specification DTD5597A Grade 60.Applications: For sealing applications where goo.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E60H Ethylene Propylene Rubber Sulphur cured, off-white Ethylene Propylene Terpolymer, 55-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States F.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E70E Ethylene Propylene Rubber Ethylene Propylene Terpolymer, 66-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace Specification DTD5597A Grade 70.Applications: For sealing applications where goo.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E70V Ethylene Propylene Rubber Peroxide cured, blue-violet Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage .. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Flex TR10; ASTM D1329 |
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer Extruded Conductive EPDM Elastomer. This is an extruded conductive elastomer engineered for resistance to harsh chemicals, specifically those associated with decontaminates for military Nuclear, Bio.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Parker Chomerics Waveguide Gaskets 877 Conductive Silicone Elastomer Gasket Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Retraction Temperature, TR10; ASTM D1329 |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with No Plasticizer MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; EN 495-5 |
Lucobit Lucofin® 1412 Polyolefin TPO Granules, Light Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; EN 495-5 |
Lucobit Lucofin® 1414 Polyolefin TPO Granules, Silk Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; EN 495-5 |
Lucobit Lucofin® 1454 Polyolefin TPO Granules, Green Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucofin® 1461 Polyolefin TPO Granules, Ice Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucolit® 1323 Polyolefin TPO Granules, Green Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucofin® 1451 Polyolefin TPO Granules, Light Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning HM-2500 CLEAR ASSEMBLY SEALANT A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning SE 4448 CV KIT PARTS A&B Excellent thermal conductivity, low volatility (D4-D10 0.03% wt), heat cure, high viscosity.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning SE 4490 CV One-part, white, non-flowing, highly filled compound, excellent thermal conductivity.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning SLYGARD® 528 FIRM GEL PARTS A&B Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | ASTM D 3575 |
Eurofoam Siliconcell 411/PLT Platinic Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning EG-3000 THIXOTROPIC GEL PARTS A&B Two-part, heat cure, thixotropic gel.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning SE 4446 CV KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning 3-4154 DIELECTRIC GEL KIT Two-part, clear, RT or heat cure.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
ATG s.r.l. IR Synthetic Polyisoprene |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
CENTROPLAST CENTROSOL Acrylonitrile butadiene Styrene copolymer CENTROSOL ABS has high rigidity and hardness even at low temperatures. It is scratch resistant, non-toxic, with high surface resistance. It is used in operation components for electrical equipment .. |