Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Denka REOMER G G3015 Thermoplastic Elastomer, For Extrusion

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Denka
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka REOMER G G3015 Thermoplastic Elastomer, For Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive distortion, rebound elasticity, etc. compared to soft PVC, and excellent bending strength and ozone resistance compared to rubberApplications[Automotive components]door moldingsweather-stripsglass run channelsside bumpersgasketsmud flapshead restsarm restssteering wheelstrimshift bar bootspedal pads[Construction material, manufacturing article home electric, appliance components]gasketsairtight materialscontainer packingpacking for vacuum cleanershosestubes[For electric wire]appliance cordscabtire
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
JIS-Z-8807
Evaporation Loss 4.0 %
4.0 %
JIS-A-5756
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
JIS-K-6301
Tensile Strength at Break 16.677 MPa
2418.8 psi
JIS-K-6723
Elongation at Break 400 %
400 %
JIS-K-6723
100% Modulus 0.0051012 GPa
0.73988 ksi
JIS-K-6723
Resilience 37
37
JIS-K-6301
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
JIS-K-6723
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 92
100°C x 120 hrs
Heating: Retention Rate of Tensile Strength, % 103
100°C x 120 hrs
Oil Resistance: Retention of Tensile Strength, % 95
JIS-K-6723
Oil Resistance: Retention Rate of Elongation, % 88
JIS-K-6723