| Category | Polymer , Adhesive , Thermoset , Silicone |
| Manufacturer | Dow Corning |
| Trade Name | SLYGARD® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Dow Corning SLYGARD® 535 THIXOTROPIC DIELECTRIC GEL.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.970 g/cc @Temperature 25.0 °C |
0.970 g/cc @Temperature 77.0 °F |
|
| Viscosity | 2900 cP | 2900 cP | dynamic |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 60 | 60 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | |
| Dielectric Strength | 11.0 kV/mm | 279 kV/in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 60.0 min @Temperature 150 °C |
1.00 hour @Temperature 302 °F |
|
| Shelf Life | 9.00 Month | 9.00 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | translucent | |
| Flowable | no | |
| Gel Hardness (Grams/Penetration) | 80 | |
| Self Leveling | yes | |
| Water Resistant | yes |