Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucobit Lucofin® 1451 Polyolefin TPO Granules, Light Blue

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Lucobit AG
Trade Name Lucofin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucobit Lucofin® 1451 Polyolefin TPO Granules, Light Blue.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhibits good toughness, superior biaxial stretchability, and flexibility even at low temperatures. It is insensitive to stress cracking and notch effects. Special stabilization provides good resistance to heat ageing and UV radiation. Lucofin is thus to a large extent resistant to weathering and ageing.Applications:• Roofing and swimming pool membranes• Construction profiles and water stops• Injection molded parts in the building sectorInformation provided by Lucobit AG
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ISO 1183
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ISO 868
Thermal Properties Metric English Comments
Minimum Service Temperature, Air <= -45.0 °C
<= -49.0 °F
Low Temperature Flexural Test; DIN 53361
Processing Properties Metric English Comments
Processing Temperature 150 - 180 °C
302 - 356 °F
Profiles
160 - 230 °C
320 - 446 °F
Membranes
160 - 240 °C
320 - 464 °F
Coatings
Melt Temperature 160 - 220 °C
320 - 428 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F