| Category | Polymer , Adhesive , Thermoset , Silicone |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Dow Corning 3-4680 SILICONE GEL KIT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.970 g/cc @Temperature 25.0 °C |
0.970 g/cc @Temperature 77.0 °F |
|
| Viscosity | 265 cP | 265 cP | dynamic |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | >= 65 | >= 65 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 3.60e+15 ohm-cm | 3.60e+15 ohm-cm | |
| Dielectric Constant | 2.75 @Frequency 100 Hz |
2.75 @Frequency 100 Hz |
|
| 2.75 @Frequency 100000 Hz |
2.75 @Frequency 100000 Hz |
||
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
| Dissipation Factor | 0.00010 @Frequency 100000 Hz |
0.00010 @Frequency 100000 Hz |
|
| <= 0.0010 @Frequency 100 Hz |
<= 0.0010 @Frequency 100 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 1.50 min @Temperature 125 °C |
0.0250 hour @Temperature 257 °F |
|
| 15.0 - 30.0 min @Temperature 22.0 °C |
0.250 - 0.500 hour @Temperature 71.6 °F |
||
| Shelf Life | 12.0 Month | 12.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | transparent | |
| Color | blue | |
| Flowable | yes | |
| Gel Hardness (Grams/Penetration) | 85 | |
| Self Leveling | yes | |
| Water Resistant | yes | |
| Working Time (min) | <10 |