| Category | Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Dow Corning SE 738 SILICONE RTV.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.05 g/cc @Temperature 25.0 °C |
1.05 g/cc @Temperature 77.0 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 33 | 33 | |
| Tensile Strength, Ultimate | 2.48 MPa | 360 psi | |
| Elongation at Break | 410 % | 410 % | |
| Shear Strength | 0.552 MPa | 80.0 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 200 °C | 392 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 3.00e+15 ohm-cm | 3.00e+15 ohm-cm | |
| Dielectric Strength | 19.7 kV/mm | 500 kV/in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 4320 min @Temperature 22.0 °C |
72.0 hour @Temperature 71.6 °F |
|
| Shelf Life | 24.0 Month | 24.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | white | |
| Flowable | yes | |
| Water Resistant | yes |