Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate Butyrate, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and ToysProcessing: Injection Molding (Melt Temperature: 445°F, Mold Temperature: 135°F)Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 1.4 %
1.4 %
(24 hr); ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.9 MPa
5210 psi
ASTM D638
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Flexural Yield Strength 37.2 MPa
5400 psi
ASTM D790
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 2.56 J/cm
4.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 229 °C
444 °F
Injection
Mold Temperature 57.0 °C
135 °F