Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

C.O.I.M. LARIPUR® LPR5450 Modified Ester Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer , Polyurethane, TP
Manufacturer C.O.I.M. S.p.A.
Trade Name Laripur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. LARIPUR® LPR5450 Modified Ester Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGreat flexibility with constancy at temperature variationsGood compression resistanceGood water and light resistanceGood resistance to oils, fats and to many types of solventsSeries 50 Modified Ester: These products are obtained by homogeneously incorporating a small amount of raw material of unique chemical composition to the products of Series 25. They combine a high level of hardness with excellent cold impact resistance.Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength, Yield 60.8 MPa
8820 psi
ASTM D412
Elongation at Break 450 %
450 %
ASTM D412
50% Modulus 0.0116 GPa
1.68 ksi
ASTM D412
100% Modulus 0.0141 GPa
2.05 ksi
ASTM D412
300% Modulus 0.0364 GPa
5.28 ksi
ASTM D412
Flexural Modulus 0.159 GPa
23.1 ksi
ASTM D790
Tear Strength 150 kN/m
856 pli
ASTM D624
Abrasion 40
40
mm3, Abrasion Loss; DIN 53516
Torsional Stiffness 37.0 MPa
5370 psi
+20°C; ASTM D1043
170 MPa
24700 psi
-20°C; ASTM D1043
Thermal Properties Metric English Comments
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Copyright © lookpolymers.com All Rights Reserved