Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 108 °C | 226 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate A, ASTM D1525 |
Plaskolite West Optix® CA-927 G HF Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: A high flow, impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven time.. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Americas Styrenics Styron® 663 Polystyrene
(discontinued **) STYRON® 663 general purpose polystyrene resin is an additive free resin with excellent strength, clarity, and high heat resistance. When used unmodified for the manufacture of food contact articles.. |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D1525 |
Eastman E6837-539A Polyethylene
(discontinued **) PolyethyleneE6837-539A is used in various injection molding applications including closures for containers or extrusion coating for high stiffness. It has good processability. This product may be us.. |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D1525 |
Polimeri Europa SINKRAL B532 ABS, Very High Impact
(discontinued **) Very high impact; injection/extrusion grade.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line. |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D1525/A |
Gichem GILAC C120/T Acrylonitrile Butadiene Styrene
(discontinued **) ABS with excellent thermal properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Vicat Softening Point | 108 °C | 226 °F | Softening Point, R&B; ASTM E-28 |
ExxonMobil Escorene® UL-7740 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Vicat Softening Point | 108 °C | 226 °F | ISO 306A |
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Vicat Softening Point | 108 °C @Load 5.00 kg |
226 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate B (120°C/h); ASTM D1525 |
Techmer ES Elastoblend® PA12 CL Availability: North AmericaForms: PelletsAppearance: Clear/TransparentInformation provided by TP Composites, Inc. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Asia Pacific) PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 108 °C | 226 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® UF-1013 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 108 °C | 226 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SR-0320BM ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 108 °C | 226 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® WR-9370 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 108 °C | 226 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Styron Magnum™ 2620 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Styron Magnum™ 585 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 108 °C | 226 °F | |
Styron Magnum™ 9450P ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East) XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C |
|||
Vicat Softening Point | 108 °C | 226 °F | ISO 306 |
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D1525 |
TPI Porene® AS 121 PC (Blue) General Purpose SAN Porene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymers. |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D1525 |
Ashley Polymers Ashlene® ABS Resin 223 Medium impact, medium flow, matte finish. Suitable for general purpose injection molding.Data provided by the manufacturer |
|||
Vicat Softening Point | 108 °C | 226 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron HR-60 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D1525 |
Plaskolite West Optix® CA-1000 E Impact Modified Acrylic Resin Extrusion Grade Pellets. Excellent blend stock material for impact applications. |
|||
Vicat Softening Point | 108 °C | 226 °F | Rate A, ASTM D1525 |
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resi.. |
|||
Vicat Softening Point | 108 °C | 226 °F | ASTM D-1525 |
Plaskolite West Optix® CP - 927 GHF High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 108 °C | 226 °F | ISO 306A |
Lucite International Diakon® ST45G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |