Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 120 °C @Load 5.001 kg |
248 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 65H PC/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 120 °C @Load 5.001 kg |
248 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525/A |
Gichem GIBLEND E45400 Polycarbonate / ABS
(discontinued **) Polycarbonate and ABS blend, high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
Hyosung Topilene C600M PP C600M Film Grade Butane Random CopolymerApplications: Metallizing CPPCharacteristics:Low sealProcessabilityInformation provided by Hyosung Corporation |
|||
Vicat Softening Point | 120 °C | 248 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® C CM 406 FD C CM 406 Polycarbonate/ABS Blend (European Grade) Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 120 °C | 248 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
Iran Petrochemical (PCC) 6070EA High Density Polyethylene HD6070EA is a high density polyethylene with a narrow molecular weight distribution. It is suitable for a wide range of injection molding applications. This grade has following characteristics: easy.. |
|||
Vicat Softening Point | 120 °C @Load 5.10 kg |
248 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Pocan® C 1202 000000 PET + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL SE100 PPE+HIPS (Europe-Africa-Middle East) NORYL® SE100 is an unfilled, flame retardant material with a Vicat B/120 of 120°C. It has a UL-94 flammability rating V1 @ 1.47 mm, and is halogen free according to VDE/DIN 472 part 815. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Europe-Africa-Middle East) Unreinforced PBT+PC alloy. Improved retention of mechanical properties under UV. Excellent low temperature/chemical |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Vicat Softening Point | 120 °C | 248 °F | VST/A/50; ISO 306 |
Styrolution Luran® S KR 2858 GS Colored 15% Glass Filled ASA Description: Glass-reinforced grade with high stiffness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 120 °C | 248 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL IN120 PPE+HIPS (Europe-Africa-Middle East) NORYL IN120 is an unfilled material with a Vicat B/120 of 125 °C according ISO 306. NORYL IN120 has been developed for the interior automotive |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL N110S PPE+HIPS (Europe-Africa-Middle East) NORYL N110S is an unfilled material with a Vicat B/120 of 115 ?C according ISO 306. NORYL N110S cust spec 1977 has been listed for potable water |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL PX1112 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1112 is an unfilled medium heat resistant material. This grade offers improved impact resistance to meet the ECE-dashboard standard. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® XD1575S PBT+PC (Europe-Africa-Middle East) XENOY XD1575S is a high flow PC+PBT blend with good impact properties and good resistance to occasional solvent and gasoline contact. XENOY XD1575S has been specially developed for coated exterior b.. |
|||
Vicat Softening Point | <= 120 °C | <= 248 °F | |
Sibur Discar-L PC/ABS Compositional Polymer Composition material PC/ABS with high shock resistance, thermal, light, and atmospheric resistance for structural parts of technical purpose and parts for internal finishing of automobiles. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Noryl EN110 PPE+HIPS (Europe-Africa-Middle East) NORYL EN110 is an extrusion material with a Vicat B/120 of 115°C according ISO 306. NORYL EN110 is a standard extrusion grade for applications where medium temperature resistance is required.This.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL N110 PPE+HIPS (Europe-Africa-Middle East) NORYL N110 is an unfilled material, with a Vicat B/120 of 115 °C according ISO 306. NORYL N110 has medium temperature resistance and good |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM-D1525 |
Polyram RamLloy PBB101 PC/ABS alloy, Injection Molding PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Vicat Softening Point | 120 °C | 248 °F | Loading 1, Rate A; ASTM D-1525 |
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren.. |
|||
Vicat Softening Point | 120 °C | 248 °F | 50N; ISO 306 |
Denka MALECCA K-300 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A (50°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hypel® PEHD30/.950 HDPE Available in North America Features: High DensityRoHS Compliant Form: Pellets Information provided by Entec |
|||
Vicat Softening Point | 120 °C @Load 5.10 kg |
248 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecotek® BC43 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade Information provided by Eurotec® |
|||
Vicat Softening Point | 120 °C | 248 °F | 49 N; ISO 306 |
A.D. Compound Adene NCZA Homopolymer 70% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
NOVA Chemicals Sclair® 35BPM MDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2715 HDPE Injection Molding Resin
(discontinued **) Features: Excellent low temperature impact strength, good balance of toughness and stiffness, low odor.Applications: Thin walled food containers and lids, frozen and refrigerated containers.Data pro.. |