| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Xenoy® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
| Density | 1.23 g/cc | 0.0444 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.150 % | 0.150 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.50 % | 0.50 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 266 °C |
26 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
| Melt Index of Compound | 25 g/10 min @Load 5.00 kg, Temperature 265 °C |
25 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D638 |
| 51.0 MPa | 7400 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
| 62.0 MPa | 8990 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 110 % | 110 % | Type I, 50 mm/min; ASTM D638 |
| 110 % | 110 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 5.0 % | 5.0 % | Type I, 50 mm/min; ASTM D638 |
| 5.0 % | 5.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.25 GPa | 326 ksi | 1 mm/min; ISO 527 |
| 2.55 GPa | 370 ksi | 50 mm/min; ASTM D638 | |
| Flexural Yield Strength | 87.0 MPa | 12600 psi | 2 mm/min; ISO 178 |
| 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.18 GPa | 316 ksi | 2 mm/min; ISO 178 |
| 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
| 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 50.0 kJ/m² | 23.8 ft-lb/in² | 80*10*4; ISO 180/1A |
| 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 71.0 J @Temperature 23.0 °C |
52.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 75.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 101 °C @Thickness 3.20 mm |
214 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 87.0 °C @Thickness 3.20 mm |
189 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| 88.0 °C @Thickness 6.40 mm |
190 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
| 124 °C | 255 °F | Rate B/120; ISO 306 | |
| 135 °C | 275 °F | Rate B/50; ASTM D1525 |