| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) | 
| Manufacturer | Eurotec | 
| Trade Name | Tecotek® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Eurotec® Tecotek® BC43 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527 | 
| Elongation at Break | >= 50 % | >= 50 % | ISO 527 | 
| Tensile Modulus | 2.25 GPa | 326 ksi | ISO 527 | 
| Izod Impact, Notched (ISO) |           20.0           kJ/m²           @Temperature -30.0 °C  | 
                  9.52           ft-lb/in²           @Temperature -22.0 °F  | 
        ISO 180/1A | 
|           35.0           kJ/m²           @Temperature 23.0 °C  | 
                  16.7           ft-lb/in²           @Temperature 73.4 °F  | 
        ISO 180/1A | |
| Izod Impact, Unnotched (ISO) |           NB                     @Temperature 23.0 °C  | 
                  NB                     @Temperature 73.4 °F  | 
        ISO 180/1U | 
|           NB                     @Temperature -30.0 °C  | 
                  NB                     @Temperature -22.0 °F  | 
        ISO 180/1U | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | ISO 75 | 
| Vicat Softening Point |           120           °C           @Load 5.10 kg  | 
                  248           °F           @Load 11.2 lb  | 
        ISO 306 | 
| Flammability, UL94 |           HB                     @Thickness 0.750 mm  | 
                  HB                     @Thickness 0.0295 in  | 
        |
|           HB                     @Thickness 1.60 mm  | 
                  HB                     @Thickness 0.0630 in  | 
        
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 | 
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Processing Temperature | 240 - 260 °C | 464 - 500 °F | |
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat | 
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
| Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | |
| Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
| Hold Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Medium - Fast |