Mechanical Properties Metric English Comments
Flexural Strength 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Rynite® FR515 BK507 PET  (Unverified Data**)
Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr..
Flexural Strength 160 MPa

@Temperature 175 °C
23200 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Flexural Strength 160 MPa

@Temperature 125 °C
23200 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
Flexural Strength 160 MPa

@Thickness 1.57 mm
23200 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP192 Synthetic Fabric  (discontinued **)
Description: 8 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high tempe..
Flexural Strength 160 MPa

@Strain 6.30 %
23200 psi

@Strain 6.30 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS.
Flexural Strength 160 MPa

@Strain 5.00 %
23200 psi

@Strain 5.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 160 MPa

@Strain 5.10 %
23200 psi

@Strain 5.10 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber
PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS.
Flexural Strength 160 MPa

@Temperature -40.0 °C
23200 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 160 MPa

@Temperature 80.0 °C
23200 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.6%); ASTM-D790
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 160 MPa

@Temperature -40.0 °C
23200 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 160 MPa

@Temperature 80.0 °C
23200 psi

@Temperature 176 °F
Practical Use (Water Absorption 1.0%); ASTM-D790
Toyobo GLAMIDE® TY-791GT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 160 MPa

@Temperature -40.0 °C
23200 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 160 MPa

@Thickness >=200 mm
23200 psi

@Thickness >=7.87 in
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr..
Flexural Strength 160 MPa

@Treatment Temp. 50.0 °C,
Time 3600 sec
23200 psi

@Treatment Temp. 122 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..
Flexural Strength >= 160 MPa

@Temperature 150 °C
>= 23200 psi

@Temperature 302 °F
Perpendicular to laminations; IEC 1212-2 5.1
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet
Flexural Strength >= 160 MPa

@Temperature 150 °C
>= 23200 psi

@Temperature 302 °F
Perpendicular to laminations; IEC 1212-2 5.1
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet
Flexural Strength 160 MPa

@Temperature 125 °C
23200 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 150FC30 Easy Flow