| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP Faradex ES003DE PEI
LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP FARADEX ES003E PEI
LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding.
|
|||
| Flexural Modulus |
4.31
GPa <br>@Thickness 3.20 mm
|
626
ksi <br>@Thickness 0.126 in
|
1.3mm/min; ASTM D790 |
|
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose
Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
|
|||
| Flexural Modulus |
4.31
GPa <br>@Thickness 3.20 mm
|
626
ksi <br>@Thickness 0.126 in
|
2.8mm/min; ASTM D790 |
|
LG Chemical LUMID HI2152A(W) PA6+GF15%, High Impact
Feature: Injection Molding, PA6+GF15%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical
|
|||
| Flexural Modulus |
4.31
GPa <br>@Thickness 3.20 mm
|
626
ksi <br>@Thickness 0.126 in
|
1.3mm/min; ASTM D790 |
|
LG Chemical Lupox® SG3250M PBT+PET+MF25%
Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical
|
|||
| Flexural Modulus |
4.31
GPa <br>@Thickness 3.20 mm
|
626
ksi <br>@Thickness 0.126 in
|
10mm/min; ASTM D790 |
|
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an..
|
|||
| Flexural Modulus |
4.31
GPa <br>@Thickness 6.40 mm
|
626
ksi <br>@Thickness 0.252 in
|
1.3mm/min; ASTM D790 |
|
LG Chemical LUPOL GP3400 PP+MF40%
Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Techmer ES Elastoblend® PA6/6 GF14 IM HS L BK 14% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Techmer ES HiFill FR® ABS GF10 FR 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, I..
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Techmer ES HiFill® ABS GF10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Techmer ES HiFill® ABS GF10 LE 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Techmer ES HiFill® PP GF20 CC HF 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High FlowInformation provided by ..
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically Coupled and Low ExtractablesInformation provided by TP Composites, ..
|
|||
| Flexural Modulus | 4.31 GPa | 626 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact
High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 4.31 GPa | 626 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Infino® LB-3150GW PC, 15% Glass Filled High Impact
High-impact resistant PC/GF that can be used for middle mold frame of LCD TVInformation provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP WF002 PBT
LNP* THERMOCOMP* WF002 is a compound based on PBT containing 10% Glass Fiber.
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | 1% Secant; ASTM D790 |
|
Washington Penn Homopolymer Polypropylene 27% Glass Reinforced
Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. ..
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy
Data provided by Clariant Masterbatches
|
|||
| Flexural Modulus | 4.31 GPa | 625 ksi | ASTM D790 |
|
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber
Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S..
|
|||