Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 4.20 GPa @Temperature 23.0 °C |
609 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B43^ D F15 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing Modified copolymer PP for injection molding, reinforced with 30% glass fiber, improved flowing. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Informatio.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | |
Plastcom SLOVAMID 6 GF 15 MI/2 PA6, 15% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Flexural Modulus | 4.20 GPa @Temperature 90.0 °C |
609 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Grupo Repol Dinalon® B1S25 G10B20 PA6 10% Glass Fiber, 20% Glass Beads Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ASTM D790 |
LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
Ineos ABS Lustran® ABS 150G10 10% Glass Fiber Reinforced Grade |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Solvay TECHNYL® A 218C V10 PA66, 10% glass fiber, DRY Description: TECHNYL® A 218C V10 is a polyamide 66, reinforced with 10% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: Due to specially.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178-93 |
Wellman Wellamid® T512-BK 15% Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6 Description: Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6Information provided by Wellman. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
Eurostar Starpylen MF007AS PP, Glass Fiber Filled, Injection Molded Starpylen MF007AS is a Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO Data |
BASF Ultradur B 4300 G2 BK5110 10% Glass Filled PBT Ultradur B 4300 G2 BK5110 is a pigmented black, easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO Data |
BASF Ultramid® NFX-0102 NF2004 30% Glass Filled PA66 (Dry) Ultramid NFX-0102 NF2004 is a heat stabilized, 30% glass bead PA66 injection molding grade. It is especially formulated for low warp, increased stiffness and excellent dimensional stability. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2.6 mm/min; ASTM D790 |
BLUESTAR LXS 314 G20 PPE-HIPS, 20% Glass Filled Typical Applications: Water industrial partsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | ISO 178 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Flexural Modulus | 4.20 GPa | 609 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |