Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.20 GPa | 1330 ksi | Tangent; ISO 178 |
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f.. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC LNP* LUBRICOMP* DFL369XF is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | |
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ISO 178 |
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding specially stabilized to improve its resistance automotive cooling liquids.Available in: Europe and Latin Americ.. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ISO 178 |
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This .. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 126F6RY01 Nylon 6, 30% Glass Fiber SAXAMID 126F6RY01 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ISO 178 |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ASTM D790 |
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ASTM D790 |
Plenco 4527 Phenolic, Granular, Transfer Molded PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under.. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ISO 178 |
Polyplastics Duranex® 6300T Polybutylene Terephthalate (PBT), Low friction, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ISO 178 |
Polyplastics FR-PET® BN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ISO 178 |
Polyplastics FR-PET® CN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ASTM-D790 |
Polyram PlusTek PA309G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, UV stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ASTM-D790 |
Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteristi.. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ISO 178 |
Unitika A1025GO PA6, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | dry; ISO 178 |
DSM Novamid® 1010GH30 NAT PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | dry; ISO 178 |
DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | dry; ISO 178 |
DSM Novamid® 1017GH33 BK701 PA6-GF33 33% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 125 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific) LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ASTM D790 |
Plenco 1506 Polyester, Briquette, Injection Molded PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop.. |
|||
Flexural Modulus | 9.20 GPa | 1330 ksi | ASTM D790 |
Plenco 7697 Phenolic, Granular, Compression Molded PLENCO 07697 is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for automotive pulleys. PLENCO 07697 is the same formulation as VALITE 697-A.Inform.. |