Material Notes:
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00732 is available in a wide range of colors.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.36 %
0.36 %
ASTM D570
Linear Mold Shrinkage 0.0054 cm/cm
0.0054 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 86
86
ASTM D785
Tensile Strength, Ultimate 76.0 MPa
11000 psi
ASTM D638
Elongation at Break 0.88 %
0.88 %
ASTM D638
Tensile Modulus 9.20 GPa
1330 ksi
ASTM D638
Flexural Strength 108 MPa
15700 psi
ASTM D790
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
Compressive Strength 204 MPa
29600 psi
ASTM D695
Izod Impact, Notched 0.206 J/cm
0.386 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.221 J/cm²
1.05 ft-lb/in²
ASTM D256
Impact 118
118
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.510 W/m-K

@Temperature 100 °C
3.54 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 150 °C
302 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 197 °C
387 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.610 mm
V-0

@Thickness 0.0240 in
Oxygen Index 33 %
33 %
ASTM D2863
Shrinkage 0.83 %
0.83 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.50e+13 ohm-cm
3.50e+13 ohm-cm
ASTM D247
Dielectric Constant 6.8
6.8
ASTM D150
Dielectric Strength 9.80 kV/mm
249 kV/in
Step by Step; ASTM D149
12.9 kV/mm
328 kV/in
Short Time; ASTM D149
Dissipation Factor 0.051
0.051
ASTM D150
Arc Resistance 185 sec
185 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638