Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.80 GPa | 1130 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Opnyl OP66GF33 Nylon 66, 33% Glass Reinforced, Conditioned Nylon 66 - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the .. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO 178 |
Nilit FRIANYL A63 GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO 178 |
Nilit RECONYL B GV30 Recycled nylon 6 for injection molding, 30% glass fiber reinforced Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.80 GPa @Temperature 23.0 °C |
1130 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D311 GF30 PBT, Glass-Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO 178 |
Nilit FRIANYL A63 H-GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ASTM D790 |
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded
(discontinued **) This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch.. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | 2mm/min; ASTM D790 |
Kingfa JE2-R2G20 Glass Fiber Reinforced ABS/PBT Alloy Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a.. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | |
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | 2mm/min; ASTM D790 |
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose) Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | 2mm/min; ASTM D790 |
Kingfa PA6-M20G16 20% Glass & 16% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240U PP SABIC® PPcompound G3240U is a general purpose, 40% glass filled, chemically coupled, heat stabilized and UV stabilized homopolymer polypropylene compound. The IMDS ID is 209768078. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON WEF32ISP PBT (Europe-Africa-Middle East) LNP * Stat-kon* WEF32ISP is a compound based on Polybutylene Terephalate resin containing Glass Fiber and Carbon Fiber. Added features include High Impact, Heat Stabilized and Electrically Conduct.. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP BF006 SAN (Europe-Africa-Middle East) LNP* THERMOCOMP* BF006 is a compound based on Styrene Acrylonitrile resin containing Glass Fiber. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP QF006 PA 6/10 LNP THERMOCOMP* QF006 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON MV008SU PP LNP VERTON* MV008SU is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO 178 |
Polyram PlusTek RA331G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced 30% Glass-fiber reinforced Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ASTM D790 |
Plenco 4301 Phenolic, Granular, Injection Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ASTM D790, ISO 178 |
EPICHEM Epinyl PA 6 GF 30 H Polyamide 6, 30% Glass, Heat Stabilized Characteristics: medium viscosity, 30% glass fibre, heat stabilized |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ASTM D790, ISO 178 |
EPICHEM Epinyl PA 6 GF 30 Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre, excellent mechanical properties |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO 178 |
Eurostar Star L PA6 30V D61 PA6, Glass Filled, Injection Molding Star L PA6 30V D61 is a PTFE/Silicone Oil Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO 178 |
CENTROPLAST CENTRODAL GF Polyoxymethylene 30% glass fiber This material has good hot water resistance and sliding properties. Its applications include seals, scrapers and chain guides, and toothed wheels and rollers.Information provided by CENTROPLAST Eng.. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO Data |
BASF Ultramid® B3GM35 BKQ649 23220 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid B3GM35 BKQ649 23220 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade. |
|||
Flexural Modulus | 7.80 GPa | 1130 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific) LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |