Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
Nilit FRIANYL B63 W-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
PolyOne Nymax™ GF 1800 35 HS Natural Polyamide 612 (Nylon 612) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
Shell Carilon® DB6G6A10 Polyketone, 30% Glass-Reinforced General-Purpose Injection Molding Grade
(discontinue Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G6A10 is a 30 percent short glass-fiber-reinforced, general purpose injection molding grade, wit.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
Nilit FRIANYL B63 GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
Grupo Repol Dinalon® B1S25 G25XV0 PA6 25% Glass Fiber V0 Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL25ES PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL25ES is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY RF206AXH PA 66 LNP LUBRILOY* RF206AXH is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material include: Wear Resistant, Healthcare. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® K4560 PBT 30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF006ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2mm/min; ISO 178 |
Teijin Panlite® BN-8110R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WFB44 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WFB44 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Glass Bead. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
Solvay TECHNYL® AR 218 V25 Nylon 66, 25% glass fiber, DRY Description: Polyamide PA66 reinforced with 25% of glass fiber, heat stabilized, containing recycled material.Available in: Europe and North AmericaProduct Applications: TECHNYL® AR 218 V25 BLACK.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178-93 |
Wellman EcoLon® MR1660-BK1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178-93 |
Wellman Wellamid® MRGF30/10 42H-GY1 Nylon 6, 30% Mineral and 10% Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
Toyobo T-750 Nylon, Painting Grade Key Feature: Glass fiber and mineral reinforced, high heat distortion gradesInformation provided by Toyobo Co., Ltd |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
Polyram PlusTek RA301G5 Nylon 6.6 for Injection Molding, 25% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 25% glass fibers reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide RF005S PA66, 25% Glass Fiber, Injection Molded Starflam RF005S is a 25% Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWUVCP 25% Mineral and 15% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ISO Data |
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106 is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The com.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
Ashley Polymers Ashlene® 630-33GU Nylon 6, 33% Glass Reinforced Nylon 6, 33% glass reinforced resin, utility grade. Also available: 630S - 33GU Heat Stabilized, 630 - 33GBU Black, 630S - 33GBU Black with H.S.Data provided by the manufacturer |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
Ashley Polymers Ashlene® 520-33GU Nylon 66, 33% Glass Reinforced Nylon 66, 33% glass reinforced resin, utility grade for non-critical applications. Also available: 520S - 33GU Heat Stabilized, 520 - 33GBU Black, 520S - 33GBU Black with H.S.Data provided by the m.. |
|||
Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
Ashley Polymers Ashlene® P266 PPO, 30% Glass Reinforced A general purpose, 30% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer |