Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | Valox® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics Valox® K4560 PBT.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
Linear Mold Shrinkage, Transverse | 0.010 - 0.012 cm/cm @Thickness 3.20 mm |
0.010 - 0.012 in/in @Thickness 0.126 in |
SABIC Method |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 96.0 MPa | 13900 psi | Type I, 50 mm/min; ASTM D638 |
102 MPa | 14800 psi | Type I, 5 mm/min; ASTM D638 | |
107 MPa | 15500 psi | Type I, 5 mm/min; ASTM D638 | |
110 MPa | 16000 psi | Type I, 5 mm/min; ASTM D638 | |
112 MPa | 16200 psi | Type I, 5 mm/min; ASTM D638 | |
115 MPa | 16700 psi | Type I, 5 mm/min; ASTM D638 | |
Tensile Strength, Yield | 112 MPa | 16200 psi | Type I, 5 mm/min; ASTM D638 |
Elongation at Break | 2.2 % | 2.2 % | Type I, 5 mm/min; ASTM D638 |
2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D638 | |
3.0 % | 3.0 % | Type I, 5 mm/min; ASTM D638 | |
4.0 % | 4.0 % | Flexural Strain, 1.3 mm/min, 50 mm span; ASTM D790 | |
4.0 % | 4.0 % | Type I, 5 mm/min; ASTM D638 | |
4.2 % | 4.2 % | Flexural Strain, 1.3 mm/min, 50 mm span; ASTM D790 | |
4.2 % | 4.2 % | Flexural Strain, 1.3 mm/min, 50 mm span; ASTM D790 | |
4.5 % | 4.5 % | Flexural Strain, 1.3 mm/min, 50 mm span; ASTM D790 | |
Elongation at Yield | 3.0 % | 3.0 % | Type I, 5 mm/min; ASTM D638 |
4.0 % | 4.0 % | Type I, 5 mm/min; ASTM D638 | |
Tensile Modulus | 8.84 GPa | 1280 ksi | 5 mm/min; ASTM D638 |
Flexural Strength | 173 MPa | 25100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Flexural Modulus | 7.10 GPa | 1030 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
7.20 GPa | 1040 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
7.40 GPa | 1070 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
7.50 GPa | 1090 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
8.00 GPa | 1160 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
Izod Impact, Unnotched | 8.17 J/cm | 15.3 ft-lb/in | ASTM D4812 |
Dart Drop, Total Energy | 6.00 J | 4.43 ft-lb | ASTM D3763 |
7.00 J | 5.16 ft-lb | ASTM D3763 | |
8.00 J | 5.90 ft-lb | ASTM D3763 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 220 °C @Thickness 3.20 mm |
428 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 200 °C @Thickness 3.20 mm |
392 °F @Thickness 0.126 in |
unannealed; ASTM D648 |