Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Nylene® PA6 Glass/Mineral Filled 7115 HS Nylon 6 15% Glass; 25% Mineral; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ISO 178, ASTM D790 |
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6 Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH
(d AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Idemitsu Kosan Xarec® N WA 7010 SPS, 10% Glass Filled
(discontinued **) Crystalline Polymer Blend, Glass Filled. Used in Automotive Electronics applications. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DCL32 PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DCL32 is a compound based on Polycarbonate resin contqaining Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | Average value: 6.90 GPa Grade Count:4 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Plenco 5440 Black General Purpose Phenolic Molding Compound
(discontinued **) Plaslok 5440 is the replacement material for the former Union Carbide BMRS-5440. It is a two-stage, phenolic molding compound that has been successfully formulated to accommodate a very wide range .. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Plenco 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Global 508 30% Glass Filled PBT Gray Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | |
Haysite ETS Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A NEMA GPO-1 economy grade fiberglass mat reinforced thermoset polyester molded sheet. ETS is an IEEE Class B 130ºC electrical/160ºC mechanical material with good punching characteristics. Typ.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Sumitomo Bakelite North America 775 CAF Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | Conditioned; ISO 178 |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ISO 178 |
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Plenco 2535 Phenolic, Granular, Injection Molded PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Toyobo Vylopet® EMC615 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: electrical and electronic componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Ashley Polymers Ashlene® 68MG Nylon 66, Glass/Mineral reinforced A glass/mineral reinforced nylon offering excellent dimensional stability and rigidity.Data provided by the manufacturer |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Chem Polymer Chemlon 109-33 G Nylon 66, 33% Glass Fiber Reinforced A highly toughened 33% glass fiber reinforced nylon 66 developed for applications requiring stiffness, creep resistance and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Chem Polymer Chemlon 233 GI Nylon 6, 33% Glass Fiber Reinforced A 33% glass fiber reinforced, impact modified nylon 6 offering a combination of creep resistance, stiffness and toughness over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Po.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 124 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Adell AT-17 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced 6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 33% Glass Reinforced.Data provided by the manufacturer |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
PolyOne Stat-Tech™ RA-06CF-07GF/000 EM Polyarylsulfone - 7% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications - Flow Enhanced Grade Data provided by PolyOne. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Custom Resins Norpex® GF3 PPE (Polyphenylene Ether), 30% Glass Filled
(discontinued **) Properties for dry as molded samples.Data provided by the manufacturer |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Plaslok 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 302 is a two-stage, woodflour and flo.. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Plaslok 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
Plaslok 204 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 204 is a two-stage, woodflour and min.. |