| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled |
| Manufacturer | Global Polymers Corporation |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Global 508 30% Glass Filled PBT Gray.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 |
| Water Absorption | 0.060 % | 0.060 % | 24 hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 110 MPa | 16000 psi | ASTM D638 |
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
| Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 23.0 µm/m-°C @Temperature 20.0 °C |
12.8 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 257 °C | 495 °F | |
| Mold Temperature | 76.0 °C | 169 °F | |
| Drying Temperature | 121 °C | 250 °F |