Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS High heat PC/ABS blend offering high modulus / low CTE and good practical impact |
|||
Flexural Modulus | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D223 Q30 FR PBT, Mineral Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
Nilit FRIANYL B63 GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
PolyOne Stat-Tech™ PF-05CF/000 EM FR Flame Retardant Polysulfone - 5% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) Zytel® 80G14AHS BK099 is a 14% glass fiber reinforced, toughened, high flow, heat stabilized, black polyamide 66 resin. It offers outstanding performance in injection molding applications.Informati.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibersInformation provided by LANXESS. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2mm/min; ISO 178 |
Teijin Panlite® G-3120PH For Cameras, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 30 % of special GF and improved appearance grade.Applications:Precision machinery, electric and electronic components that need dimensional accuracy and good appearance.Information p.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PFB42U PA 6 (Europe-Africa-Middle East) LNP STARAMIDE PFB42U is a compound based on Nylon 6 resin containing Glassfiber and Glass Beads Additional features include Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-M.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MH0255A PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MH0255A is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features include; High Specific Gravity.This data was supplied by SABIC-IP for the Europe-.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RB008 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RB008 is a compound based on PA 66 resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
Tipco Tipcolene® FPT 40 NEX - 40% Talc Reinforced Polypropylene Homopolymer, Low MFI 40% Talc Reinforced PP HomopolymerApplications: Sheets, Pipes, ProfilesProcessing: ExtrusionInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
Polyram RamSter PF302G3 PBT, 15% Glass Fiber, UV Stabilized 15% Glass fiber reinforced, UV stabilized PBT for injection molding application.Information provided by Polyram. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
Ensinger Tecapeek® ID Metal Detectable Polyetheretherketone Tecapeek™ ID metal detectable polyetheretherketone, made from Victrex® PEEK 450G polymer, is formulated to reduce the risk of product contamination and allow for easy detection of fragments in the.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | DAM; ISO 178 |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) 32% Mineral Reinforced Toughened Polyamide 66 Minlon 12TA BKB124 is a 32% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont P.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PFB42U PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42U is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | cond; ISO 178 |
DSM EcoPaXX® Q-HGM24 PA410-(GF+MD)30 10% Glass Reinforced, 20% Mineral Reinforced, Heat Stabilized |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
Beijing Chemical Industry KAIFA® M109-G20 MPPO Resin 20% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2mm/min; ISO 178 |
Teijin Panlite® G-3415R Glass Fiber Reinforced Polycarbonate Resin GF 15% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS BK099 is a 14% glass fiber reinforced toughened high flow heat stabilized black polyamide 66 resin. It offers outstanding p.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH304G25 Polypropylene Homopolymer, 25% Glass Filled SAXALEN PPH304G25 is a 25% glass filled Polypropylene - Homopolymer intended for injection molding. This compound is characterized by high stiffness good impact resistance und reduced creep under lo.. |