Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.80 GPa | 406 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Uttap SF 600 Polyethersulfone Polyether Sulfone Resin-Medium Viscosity, unreinforced standard grade for Easy Injection Molding.Information provided by Ovation Polymers |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Europe-Africa-Middle East) PC+ABS, of non-chlorinated & non-brominated flame retardant with Sparkle effect.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO 178 |
Nilit FRIANYL A63 N-V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, low viscosity, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP J1000Z PES (Europe-Africa-Middle East) LNP* COLORCOMP* is a compound based on Polyethersulfone resin. Added features include: High Viscosity |
|||
Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T16020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 |
PolyOne Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46 LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO Value |
BASF Capron® 8203C Nylon 6 (Dry)
(discontinued **) Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 1-3120 N DEL 20% Talc Filled Polypropylene Homopolymer INNOPOL® CS 1-3120 B DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® BC 30 S 000000 Nylon 6 PA 6, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem DH1004F PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM-D790 |
Polyram RamTough PZ320G2 Polycarbonate, 10% Glass Fiber, Flame Retardant 10% glass fiber reinforced, flame retardant polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D 790 |
Cossa Polimeri ESTADIENE 0615 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood impact resistance, stiff, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | dry; ISO 178 |
DSM Novamid® 1011CH5KR PA6 Heat Stabilized, Easy Molding Grade |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | dry; ISO 178 |
DSM Novamid® 1013C5 PA6 Injection Molding, Easy Molding Grade |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 HWV0CP Nylon 6, Flame Protection, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO 178 |
Eurostar Staramide R1000 PA66, Injection Molded Staramide R1000 is an Unreinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 45HSB NC010 is a high viscosity heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Poly.. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 |
E-Polymers TEKAMID® TA210 LW TA210LW, Low Wear, Low Friction PA66, DAM Low wear, Low frictionInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 |
Ashley Polymers Ashlene® 520MS/520SMS Nylon 66, MoS2 Filled A general purpose Molybdenum-disulfide filled nylon resin.Data provided by the manufacturer |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | Dry; ASTM D790 |
Asahi Kasei Leona® 1700S Nylon 66 Similar to 1500 but with even higher molecular weight. Suitable for extrusion of thick-wall parts.Applications:Rods, films Information provided by Asahi Kasei |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | ISO Data |
BASF Ultramid® 1003-2 NF2002 PA66 (Dry) Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6. |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 HWCP Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 2.80 GPa | 406 ksi | DAM; ISO 178 |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |