Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.11 GPa | 306 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Europe-Africa-Middle East) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DI001L PC LNP* LUBRICOMP* DI001L is a compound based on Polycarbonate resin containing 2% Silicone. Added characteristics of this grade are: Low Extractable. |
|||
Flexural Modulus | 2.11 GPa @Thickness 3.20 mm |
306 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Flexural Modulus | 2.11 GPa @Thickness 3.20 mm |
306 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.11 GPa @Thickness 3.20 mm |
306 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY SC1004AU PC, High Impact Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.11 GPa @Thickness 3.20 mm |
306 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY SC1004L PC, High Impact Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc.. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® FD-1102 PC, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | ASTM D790 |
Samyang Tribit® 1700 PBT, Middle Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1700 is a middle viscosity grade.Informatio.. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | ASTM D790 |
Samyang Trirex® 3022PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022PJ is a general use grade.Information provided by Samyang. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | ASTM D790 |
Samyang Trirex® 3022R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022R is a general use grade with heat stabilizers and separating materials added.Appli.. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON FX91304 PE LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Flexural Modulus | 2.11 GPa @Thickness 3.20 mm |
306 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 6456 High Heat Polystyrene Characteristics High heat resistance & strength Very good flow properties Available in any dark colorsProcessing Injection moldingApplications Instrument enclosures TV components Electrical encl.. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | (tangent); ASTM D790-10A |
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC) TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products .. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | |
Zylog Hipolyene® 1532 MS Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | |
Zylog Hipolyene® 6251 Y Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | ISO 178 |
Polyram PlusTek PB845 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® X0722 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.11 GPa @Thickness 6.40 mm |
306 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron AN480V2 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Flexural Modulus | 2.11 GPa | 306 ksi | ASTM D790 |
Aaron Industries AAROLENE® AVPS HIPS 100-3 MELT 14 Virgin HIPS Resin A virgin, high impact polystyrene, natural in color, specifically designed for injection molding applications. |
|||
Flexural Modulus | 2.11 GPa @Thickness 6.40 mm |
306 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron AN480V2 Flame Retardant ABS Grade Information provided by Bhansali |