Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zylog Hipolyene® 6251 Y Thermoplastic Polyolefin & PP Compound

Category Polymer , Thermoplastic , Polyolefin , Polypropylene (PP)
Manufacturer Zylog Plastalloys
Trade Name Hipolyene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zylog Hipolyene® 6251 Y Thermoplastic Polyolefin & PP Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Melt Flow 10 g/10 min
10 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.6 MPa
2840 psi
Elongation at Break 30 %
30 %
Flexural Modulus 2.11 GPa
306 ksi
Izod Impact, Notched 1.18 J/cm
2.20 ft-lb/in
Users viewing this material also viewed the following: