Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.8 GPa | 1570 ksi | ISO 178 |
Radici Radiflam® ARV300 AE (dry) Nylon 66 PA66 Self-extinguishing glass-fiber reinforced with halogensInformation provided by Radici group. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, at 50% RH
&n AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LNP Stat-Kon® PDX-E-99689 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LNP Thermocomp® EF-1006 EM Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Flexural Modulus | 10.8 GPa | 1560 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN135HB40SIBL Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ISO 178 |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ISO 178 |
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is .. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFL28 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WFL28 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Flexural Modulus | 10.8 GPa | 1560 ksi | |
Shinil Chemical SHINCON PES Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Flexural Modulus | 10.8 GPa | 1560 ksi | |
Shinil Chemical SHINCON PES-CNT Magazine Rack Magazine Rack is used to transfer, handle, and bake lead frame or PCB substrate in semiconductor and LED packaging assembly process. Current Metal Magazine is made of anodized aluminum which is exp.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific) LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & .. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific) LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Flexural Modulus | 10.8 GPa | 1560 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-5302GR PBT, 30% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 10.8 GPa | 1560 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XI-2008F PPS/PPA, Mineral Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 10.8 GPa | 1560 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-3402F PC, 40% Glass Filled FR PC/GF material with 40% GF reinforcement that can be used in printer LSUInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP UCF22S PPA LNP* Thermocomp* UCF22S is a compound based on Polyphthalamide resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RX03013 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX03013 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | dry; ISO 178 |
DSM Akulon® K224-G8 PA6-GF40 40% Glass Reinforced |
|||
Flexural Modulus | 10.8 GPa @Temperature 23.0 °C |
1570 ksi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers VESPEL TP-8792 Polyimide DuPont Vespel TP-8792 parts are specified for mechanical, thermal, and tribological properties. TP-8792 offers excellent strength and toughness, dimensional stability, low outgassing, radiation resi.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 247 SAN, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.8 GPa | 1560 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XI-2008F PPS/PPA, Mineral Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |