Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 145 MPa
21000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 203 MPa
29400 psi
ASTM D790
Flexural Modulus 10.8 GPa
1570 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.89 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 205 - 225 °C
401 - 437 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 260 - 271 °C
500 - 520 °F