Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
PolyMirae Moplen HP620M CPP Film Grade Polypropylene Moplen HP620M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP620M is suitable for rigid core resin of CPP. Moplen HP620M res.. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
PolyMirae Moplen HP640N Injection Molding Grade Polypropylene Moplen HP640N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640N is a homopolymer particularly suitable for injection molding.. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene Moplen HP740T is a nucleated polypropylene HOMO polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP740T is a homopolymer selected by customers for use in t.. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
I. Stern HIPS SH03 High Impact Polystyrene Features:High flowExcellent toughnessExcellent processabilityApplicationsInjection moldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co. Inc. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790 |
LG Chemical LUPOL HG-3250 High Gloss Polypropylene, 25% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | |
Kraton® G1651 + PPE blend (10/90) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790 |
Hannam Chemical Hanalac 795 ABS, Pipe Grade Designed for pipe and bobbin sleeves. Excellent processability and high impact strength. Manufactured to prevent static electricity. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN173HI3R High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL GP3156F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided .. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9160 ASA, Unreinforced Used in electric goods etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | ASTM D790 |
Samyang Triloy® 130 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Flexural Modulus | 1.77 GPa | 257 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re.. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SH 03 High Impact Polystyrene Characteristics High flow Good melt strength Excellent toughness Processing MoldingApplications Gas assisted injection molding of T.V. cabinets Suitable for thin walled parts, AC grills and toys .. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 246 Toughened Polystyrene Characteristics Excellent clarity Very high toughness Deep drawability Improved thermal stabilityProcessing Extrusion ThermoformingApplications Thermoformed clear and deep draw products Rectangu.. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 266 Toughened Polystyrene CharacteristicsGood stiffness Excellent toughness High flow Excellent clarity Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric instruments .. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 556 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any color Processing Extrusion MoldingApplications T.V. Cabinets, computer monitor, printer housing Elect.. |
|||
Flexural Modulus | 1.77 GPa @Thickness 3.20 mm |
256 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 566 Flame Retardant Polystyrene Characteristics Good flow and toughness Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Available in any color Processing Extrusion MoldingApplications Large size T.V. Cabinets El.. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 6131 XF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 8515 TY Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 8005 DW Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa | 256 ksi | |
Zylog Hipolyene® 8015 FRC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron PT-45M ABS Antistatic Extrusion Grade Antistatic Cop Sleeves ApplicationInformation provided by Bhansali |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron PT-45M ABS Antistatic Extrusion Grade Antistatic Cop Sleeves ApplicationInformation provided by Bhansali |
|||
Flexural Modulus | 1.77 GPa @Thickness 6.40 mm |
256 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |