Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANPRO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use.Applications: Slit tape and monofilament for rope, twine, yarn and industrial fabrics.Advantages: Outstanding process-ability. Maximum bubble stability for slit tape production by the tubular process. Good melt stability. Low color. Low taste and odor. No plate out problems on die lips or chill rolls. Good heat-aging stability in yarn and fabric.Fabrication: Equipment - general extrusion. Techniques - standard processing for tubular and flat die tapes. Information provided by Titan ChemicalsCAS# 9003-07-0
Physical Properties Metric English Comments
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Water Absorption 0.020 %
0.020 %
after 24 hrs; ASTM D570
Base Resin Melt Index 3.0 g/10 min

@Temperature 230 °C
3.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785A
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.77 GPa
257 ksi
ASTM D790B
Izod Impact, Notched 0.382 J/cm
0.716 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648