Material Notes:
Moplen HP640N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640N is a homopolymer particularly suitable for injection molding of houseware articles, toys, packaging, closures and medical items. Moplen HP640N resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Good Transparency; High Gloss; Excellent stiffness; Good mechanical property balanceApplications: Houseware articlesInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 34.3 MPa
4980 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.77 GPa
256 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
252 °F
ASTM D648
Vicat Softening Point 157 °C
315 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 70 %
70 %
ASTM D1003