Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.38 GPa | 200 ksi | Tangent; ASTM D790 |
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.38 - 3.45 GPa | 200 - 500 ksi | ASTM D790 |
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
S&E Specialty Polymers TufGuard M™ GPP1001M-P-2986 Grey PP, Flame Retardant Application: High impact resistant, non-blooming flame retardant polypropylene compound designed for UL94 V-0 injection molding applications.Information provided by S&E Specialty Polymers |
|||
Flexural Modulus | 1.38 - 2.76 GPa | 200 - 400 ksi | ASTM D790 |
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 31% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
M. Holland Company PP204 Polypropylene Homopolymer Features: Homopolymer, Low Residuals, Good Stiffness, Low Water CarryoverApprovals: FDA 21 CFR 177.1520Information provided by M. Holland. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
ScanTube ETFE Tubing Information provided by ScanTube, Inc. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2306N Impact Copolymer Polypropylene Impact Copolymer for Compression and Injection Molded Caps and Closures Formolene® 2306N is a polypropylene copolymer formulated for compression and injection molded cap applications. It was create.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 4101O BCF Fiber Spinning Polypropylene HomopolymerApplications: Multifilament and bulk continuous filament fiber.Formolene 4101O is a low viscosity, highly isotactic polypropylene homopolymer designed primarily for multifilament and bulk.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
Total PPC 4820WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
ExxonMobil HDPE BA53-055 High Density Polyethylene Resin Product Description: BA53-055 is a high molecular weight, high density polyethylene copolymer.Availability: Latin America, North America and South America Additive: Antistatic: NoApplications: Dru.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4350P Impact Copolymer Polypropylene Description: Good balance of stiffness and impact strength, excellent organoleptic properties.Applications: Suggested uses include compounding, thin-walled injection molding.Process: Injection Moldi.. |
|||
Flexural Modulus | 1.38 - 1.66 GPa | 200 - 241 ksi | |
3D Systems Accura® 25 Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
Amco PRIMATOP HDPE 002955 Phillips Process Hexene Copolymer PRIMATOP HDPE 002955 has a high melt strength, excellent stiffness, and excellent stress crack resistance. Applications include large part blow molding resin and sheet extrusion thermoforming.Former.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
A. Schulman PP 3488-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3488-01 is a specially formulated homopolymer polypropylene designed for large appliance injection molding. This material has excellent chemical resistance in addition t.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 |
Quadrant EPP Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |
|||
Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790A |
BP Amoco Acclear® 8649X Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Developmental Grade. Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Low taste/odor, Excellent processabilityTypical applications: High clarity c.. |