Material Notes:
Features: Homopolymer, Low Residuals, Good Stiffness, Low Water CarryoverApprovals: FDA 21 CFR 177.1520Information provided by M. Holland.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Modulus 1.52 GPa
220 ksi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Form Pellets