Material Notes:
PRIMATOP HDPE 002955 has a high melt strength, excellent stiffness, and excellent stress crack resistance. Applications include large part blow molding resin and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 35 hour
35 hour
Condition B, F50; ASTM D1693
45 hour
45 hour
Condition A, F50; ASTM D1693
Melt Index of Compound 0.25 g/10 min
0.25 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
2" per min, Type IV; ASTM D638
Elongation at Break >= 600 %
>= 600 %
2" per min, Type IV; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -84.4 °C
<= -120 °F
ASTM D746