Material Notes:
Product Description: BA53-055 is a high molecular weight, high density polyethylene copolymer.Availability: Latin America, North America and South America Additive: Antistatic: NoApplications: DrumsFood packagingHeavy Gauge SheetLarge Part Blow MoldingThermoformed Parts Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D4883
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
ASTM D1963
Melt Flow <= 0.10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
<= 0.10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
5.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Break 1400 %
1400 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Tensile Impact Strength 357 kJ/m²
170 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -85.0 °C
<= -121 °F
ASTM D746